Citation: | CHEN Xiaoyu, TANG Maolin. Corrosion Rate of Non-Galvanized High-Strength Steel Wires under Different Temperature and Humidity Conditions[J]. Journal of Southwest Jiaotong University, 2018, 53(2): 253-259. doi: 10.3969/j.issn.0258-2724.2018.02.005 |
孙跃, 胡津.金属腐蚀与控制[M].哈尔滨:哈尔滨工业大学出版社, 2003:1-9.
|
BETTI R, YANEV B. Corrosion monitoring research of new york city bridges[R]. Washington D. C.: Transportation Research Board, 2013. https://trid.trb.org/view/1286050
|
National Cooperative Highway Research Program. NCHRP-Report[R]. New York: [s.n.], 2004.
|
陈小雨, 沈锐利, 张培炎.悬索桥主缆的内部检测[J].世界桥梁, 2013, 41(1):86-90. http://d.old.wanfangdata.com.cn/Periodical/gwql201301019
CHEN Xiaoyu, SHEN Ruili, ZHANG Peiyan. Internal inspection of suspension bridge main cable[J]. World Bridges, 2013, 41(1):86-90. http://d.old.wanfangdata.com.cn/Periodical/gwql201301019
|
SUZUMURA K, NAKAMURA S I. Environmental factors affecting corrosion of galvanized steel wires[J]. Journal of Materials in Civil Engineering, 2004, 16:1-7. doi: 10.1061/(ASCE)0899-1561(2004)16:1(1)
|
黎学明, 陈大华.模拟酸雨溶液中温度对桥梁索缆镀锌钢丝腐蚀行为影响[J].腐蚀科学与防护技术, 2010, 22(1):14-17. http://www.wanfangdata.com.cn/details/detail.do?_type=perio&id=CAS201303040000304935
LI Xueming, CHEN Dahua. Effect of temperature on corrosion behavior of galvanized steel bridge wires in simulated acid rain[J]. Corrosion Science and Protection Technology, 2010, 22(1):14-17. http://www.wanfangdata.com.cn/details/detail.do?_type=perio&id=CAS201303040000304935
|
杨文静, 黎学明, 周建庭.大跨度桥梁缆索模拟酸雨加速腐蚀行为研究[J].腐蚀科学与防护技术, 2011, 23(1):65-68. http://www.cnki.com.cn/Article/CJFDTotal-FSFJ201101018.htm
YANG Wenjing, LI Xueming, ZHOU Jianting. Research of accelerated corrosion behavior of long-span bridge cable simulated acid rain[J]. Corrosion Science and Protection Technology, 2011, 23(1):65-68. http://www.cnki.com.cn/Article/CJFDTotal-FSFJ201101018.htm
|
BETTI R, MARCONI G, KHAZEM D, et al. Experimental analysis of a nondestructive corrosion monitoring system for main cables of suspension bridges[J].Journal of Bridge Engineering, 2013, 18(7):653-662. doi: 10.1061/(ASCE)BE.1943-5592.0000399
|
缪长青, 尉廷华.大跨桥梁缆索钢丝腐蚀速率的研究[J].西南交通大学学报, 2014, 49(3):513-518. doi: 10.3969/j.issn.0258-2724.2014.03.022
MIAO Changing, WEI Tinghua. Corrosion rate test of cable wires of large span bridge[J]. Journal of Southwest Jiaotong University, 2014, 49(3):513-518. doi: 10.3969/j.issn.0258-2724.2014.03.022
|
CHEN Xiaoyu, TANG Maolin. Influence analysis of the corrosion factors effect on the corrosion rate of steel wires of main cable of suspension bridge[C]//IABSE Conference. Guangzhou: [s.n.], 2016: 155-163. https://www.ingentaconnect.com/content/iabse/report/2016/00000106/00000011/art00008
|
施彦彦.典型金属材料大气腐蚀的模拟电化学研究[D].杭州: 浙江大学, 2008. http://www.wanfangdata.com.cn/details/detail.do?_type=degree&id=Y1378979
|
俞明德, 沈锐利, 唐茂林, 等.西堠门大桥主缆横断面温度场研究[J].建筑科学与工程学报, 2010, 27(3):53-58. http://d.old.wanfangdata.com.cn/Periodical/xbjzgcxyxb201003010
YU Mingde, SHEN Ruili, TANG Maolin, et al. Research on temperature field of main cable section of xihoumen bridge[J]. Journal of Architecture and Civil Engineering, 2010, 27(3):53-58. http://d.old.wanfangdata.com.cn/Periodical/xbjzgcxyxb201003010
|
杨宁.大跨度悬索桥的主缆除湿防护系统[D].上海: 同济大学, 2006.
|
DOUGLAS W B, RICHARD J. Linear polarization resistance sensor using the structure as a working electrode[C]//European Conference of The Prognostics and Health Management Society. Santa Clara: [s.n.], 2014: 1-7. http://citeseerx.ist.psu.edu/viewdoc/summary?doi=10.1.1.655.3670
|
何为, 薛卫东.优化试验设计方法与数据分析[M].北京:化学工业出版社, 2012:29-284.
|